Please use this identifier to cite or link to this item: http://repositorio.unitau.br/jspui/handle/20.500.11874/2680
Full metadata record
DC FieldValueLanguage
dc.contributor.authorBarcellos, Aline Serrado de Pinhopt_BR
dc.contributor.authorMarinho, Caroline Cotespt_BR
dc.contributor.authorMiranda, Jean Soarespt_BR
dc.contributor.authorAmaral, Marinapt_BR
dc.contributor.authorShiino, Marcos Yutakapt_BR
dc.contributor.authorKimpara, Estevao Tomomitsupt_BR
dc.date.accessioned2019-09-12T16:53:37Z-
dc.date.available2019-09-12T16:53:37Z-
dc.date.issued2018-
dc.citation.volume81pt_BR
dc.citation.spage173-
dc.citation.epage177-
dc.identifier.doi10.1016/j.jmbbm.2018.02.007pt_BR
dc.identifier.issn1751-6161-
dc.identifier.issn1878-0180-
dc.identifier.urihttp://repositorio.unitau.br/jspui/handle/20.500.11874/2680-
dc.description.abstractThe aim of this study was compare the effect of two in vitro ageing protocols to intraoral aging on the flexural strength of a lithium disilicate (LD) ceramic bars with clamped ends. After polishing and crystallization, the both ends of the bars were cemented to a metallic device and subjected to mechanical cycling, thermomechanical cycling, or intraoral ageing. Ten volunteers used an intraoral device - similar to an occlusal splint with a balanced contact condition on the occlusal surface of the ceramic bar - during 8 h night time / 30 days. Both in vitro and intraoral ageing decreased the flexural residual strength of LD, with the lowest values obtained after intraoral ageing. Thus, the in vitro ageing protocols tested in this study revealed to be less deleterious than intraoral ageing of LD.en
dc.description.provenanceMade available in DSpace on 2019-09-12T16:53:37Z (GMT). No. of bitstreams: 0 Previous issue date: 2018en
dc.languageInglêspt_BR
dc.publisherElsevier Science Bv-
dc.publisher.countryHolandapt_BR
dc.relation.ispartofJournal of the Mechanical Behavior of Biomedical Materials-
dc.rightsEm verificaçãopt_BR
dc.sourceWeb of Sciencept_BR
dc.subject.otherFixed Partial Denturesen
dc.subject.otherGlass-Ceramicsen
dc.subject.otherClinical-Performanceen
dc.subject.otherFracture Strengthen
dc.subject.otherDental Ceramicsen
dc.subject.otherGold Alloyen
dc.subject.otherTitaniumen
dc.subject.otherCrownsen
dc.subject.otherHoten
dc.titleEffect of fatigue protocols on flexural strength of lithium disilicate bars with clamped-endsen
dc.typeArtigo de Periódicopt_BR
dc.identifier.wosWOS:000430772200019-
dc.description.affiliation[de Pinho Barcellos, Aline Serrado; Marinho, Caroline Cotes; Miranda, Jean Soares; Shiino, Marcos Yutaka] Univ Estadual Paulista, Inst Sci & Technol, Sao Paulo, Brazil-
dc.description.affiliation[Amaral, Marina; Kimpara, Estevao Tomomitsu] Universidade de Taubaté (Unitau), Dept Dent, Sao Paulo, Brazil-
dc.subject.wosareaEngineering, Biomedicalen
dc.subject.wosareaMaterials Science, Biomaterialsen
dc.subject.researchareaEngineeringen
dc.subject.researchareaMaterials Scienceen
Appears in Collections:Artigos de Periódicos

Files in This Item:
There are no files associated with this item.


Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.